Starting with a 2inch diameter rod of brass we would like to

Starting with a 2-inch diameter rod of brass, we would like to process 0.2-inch diameter rods that possess minimum yield strength of 40 ksi and a minimum elongation to fracture of 40%, (see the following figure). Design a process that achieves that.

Starting with a 2-inch diameter rod of brass, we would like to process 0.2-inch diameter rods that possess minimum yield strength of 40 ksi and a minimum elongation to fracture of 40%, (see the following figure). Design a process that achieves that.

120 70% Cu-30% Zn 100 Tensile strength 80 e 60 Yield strength 9 40 40 5 D 20 Elongation 0 30 Percent cold work 0 10 20 40 50 50 60

Solution

Hot extrusion to convert into smaller diametr

Cold extrusion to further elongate

Annealing for increasing the ductility

Heat treatment for increasing strength

Cold working for imcreasing fracture toughness

Starting with a 2-inch diameter rod of brass, we would like to process 0.2-inch diameter rods that possess minimum yield strength of 40 ksi and a minimum elonga